Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7442b6cce4e96d3dc4a380851e9224d8 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-50 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-12 |
filingDate |
2007-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7addc25d11133091c00800793a68ef33 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_10fc611837f4d0e00d7d291885afdd83 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_172434325c83195128e97a44851134bb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_586394e3b83f96baba2822606de35306 |
publicationDate |
2008-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2008110762-A1 |
titleOfInvention |
Electrolyte Composition and Method for the Deposition of a Zinc-Nickel Alloy Layer on a Cast Iron Or Steel Substrate |
abstract |
The present invention relates to an electrolyte composition as well as a method for the deposition of zinc-nickel alloy layers on substrates, in particular cast iron or steel substrates. The electrolyte compositions according to the invention comprise aminoacetic acid. The alloy layers deposited from the electrolyte compositions according to the invention are corrosion resistant and bright and nearly have no internal tension. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9435047-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016002804-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011195272-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104651888-A |
priorityDate |
2006-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |