Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7610cef0de1410bf21e1e54706e208a |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1216 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-28 |
filingDate |
2007-09-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4189d2fd4ffa2ea4977afaba3ee407a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a1dee5358eb58f40c8eccacdba4e3fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a5233e626f76c9c3199ca3d22aaf226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ccdf35e479e967059f3f489ecd23ec3 |
publicationDate |
2008-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2008108498-A1 |
titleOfInvention |
Method for preparing a large continuous oriented nanostructured mixed metal oxide film |
abstract |
This invention provides a general method for preparing a large oriented nanostructured mixed metal oxide (MMO) film comprising the steps of (a) preparing a highly (00l)-oriented LDH film, and (b) calcining the LDH film at a temperature of 300° C. to 1300° C. for 10 min to 36 h to obtain an oriented nanostructured MMO film. In the oriented MMO film, MMO nanoparticles are densely packed and form defect-free films which have high thermal stability. The major advantage of the present method is that it can be used for mass-production of large continuous oriented nanostructured MMO films without using any templates, lattice-matched single-crystalline substrates and/or expensive equipment, and the composition of the prepared MMO films can be readily adjusted by changing the composition of the LDHs fims as the precursor. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10906859-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11351604-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10906028-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10106482-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10105684-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111790396-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10138199-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10087355-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113278986-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10875092-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10252245-B2 |
priorityDate |
2006-11-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |