abstract |
A method for manufacturing a negative electrode for a non-aqueous electrolyte secondary battery is provided. A negative electrode precursor of the non-aqueous electrolyte secondary battery is allowed to absorb lithium ions, the negative electrode precursor includes a current collector and an active material layer formed on the current collector. The precursor is provided with an exposed portion of the current collector. In this method, a negative electrode active material layer is allowed to absorb lithium ions by electrolysis in the non-aqueous electrolyte solution. At this time, by measuring a potential of a portion immersed in the non-aqueous electrolyte solution, the exposed portion is detected and an electric current of the electrolysis is controlled. Thereby, the deposition of lithium metal on the exposed portion is suppressed. |