Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fce5ff40c7ed9aa6caebe463c9d48a6c |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K21-14 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K21-14 |
filingDate |
2007-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b704ea5397d20fa2fc6f24515e48ea3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af746f6fe2c877986df80bd2243bfc51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed1ee6b63434b316ce0bfbfc8d77217b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_398b4054067aa3788d0554bb7a1ec8dd |
publicationDate |
2008-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2008054234-A1 |
titleOfInvention |
Flame retardative resin composition |
abstract |
A nonflammable resin composition comprises (A) at least an epoxy resin with biphenyl unit or naphthyl unit; (B) at least a phenolic resin used as a hardener, wherein the phenolic resin has a skeleton formed by phenyl rings bonding directly each other without interruption, and is in an amount of 30 to 100% by weight based on total hardeners; and (C) a curing catalyst. The said nonflammable resin has an excellent flame retardancy, a good heat resistance, and an improved moldability and reliability. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008262127-A1 |
priorityDate |
2006-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |