Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e94174d1e4e9431f19b2c16ffd706181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_215813bb1ebee8a0beb2ef95b069b565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0c6cffaeed7dec0f1e4e697c7fc85e1e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T152-10495 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2300-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-3437 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2319-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L93-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2317-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2220-4893 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L19-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-04 |
filingDate |
2006-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0981566f3b6acadf117d5d67535fb3dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1526afd933dea340dea0c65916852efa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1199503794ed05bfe0c35ace9571e796 |
publicationDate |
2007-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2007299149-A1 |
titleOfInvention |
Method of making and using sorbent and filtering material from secondary waste rubber |
abstract |
A method of making a sorbent from waste rubber and a method of sorbing oil using such sorbent. Approximately two pounds of modifier is added to 100 pounds of vulcanized rubber waste, the modifier comprising a mixture by weight of (i) a slightly water-soluble organic acid having a melting point of 70° C. or higher representing 80%, (ii) quinine group bases representing 19% and (iii) 1% of an anti sliding ingredient such as colophony, running the mixture of rubber waste and modifier in a roll mill approximately six times to crush it and placing the crushed modified rubber particles in an extruder for 2-10 minutes at 120-150° C. The sorbent can then be applied to oil to sorb six times its own weight in oil. The sorbent can be re-used two more times after extracting the oil. The sorbent is also effective at filtering oil from water. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10493379-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022061408-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10456771-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011109598-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8758629-B2 |
priorityDate |
2006-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |