abstract |
A polyamide based resin film roll is provided. The polyamide based resin film roll comprising: a first sample cutout portion within 2 m from the winding end of film; and a final cutout portion within 2 m from the winding start of film, wherein when a sample cutout portion is set up in approximately every 100 m from the first sample cutout portion, in all samples cut out from each of the cutout portions, mechanical properties such as boiling water shrinkage percentage and refraction index in the thickness direction are adjusted within a given range of variation width. |