abstract |
An acrylic resin film, in which acrylic elastic particles are mixed with an acrylic resin containing glutaric anhydride units, has a total light transmittance of 91% or more, a haze value of 1.5% or less, a folding endurance value (times) of 20 or more, and a heat shrinkage rate of less than 5% at least in either the machine direction or the transverse direction in a heat shrinkage test. |