Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F297-083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F297-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-48 |
filingDate |
2005-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58dfb10fe0ba3af33fa2d64bd5633467 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0b1b58eb154f10dcbf71b54bf5ed8ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_37bf1b2eba04acdc4410dbd21d3f9df2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87a13cb3e6ce129fa205f319910ff412 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d0cfb7facad75633e4d81bfa1587125 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_772528060a1e9b9cdec7a951b0698408 |
publicationDate |
2007-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2007238828-A1 |
titleOfInvention |
Propylene Resin Composition and Molding Thereof |
abstract |
To provide a propylene resin composition excellent in both the electroconductivity and moldability and excellent in their balance, and a molded product thereof. n A propylene resin composition comprising from 50 to 98 wt % of a propylene resin having a MFR of from 5 to 300 g/10 min, and from 2 to 50 wt % of carbon black having a 24M4DBP absorption of at least 130 cm 3 /100 g, a dehydrogenation amount of at most 1.2 mg/g at 1,500° C. for 30 minutes and a crystallite size (Lc) of from 10 to 17 Å. A propylene resin molded product which is a propylene resin molded product obtained by molding such a propylene resin composition and which has a volume resistivity of from 10 2 to 10 9 Ω·cm and a MFR of from 1 to 80 g/10 min. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011014407-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10174188-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9434851-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014107274-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8217116-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113348063-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015232679-A1 |
priorityDate |
2004-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |