abstract |
The invention concerns a method for producing products and coarse iron-based powder comprising a lubricant having a crystalline melting point below 25° C., a viscosity (η) at 40° C. above 15 mPas and wherein said viscosity is temperature dependent according to the following formula: 10 log η=k/T+C wherein the slope k is preferably above 800, T is temperature in Kelvin and C is a constant, in an amount between 0.05 and 0.4%. |