abstract |
A method of manufacturing a molecular sieve of the MCM-22 family, said method comprising the steps of (a) providing a mixture comprising at least one source of ions of tetravalent element, at least one source of alkali metal hydroxide, at least one directing-agent (R), water, and optionally at least one source of ions of trivalent element, said mixture having the following mole composition:n Y:X 2 =10 to infinity H 2 O:Y=1 to 20 OH − :Y=0.001 to 2 M + :Y=0.001 to 2 R:Y=0.001 to 0.34n nwherein Y is a tetravalent element, X is a trivalent element, M is an alkali metal; (b) treating said mixture at crystallization conditions for less than 72 hr to form a treated mixture having said molecular sieve, wherein said crystallization conditions comprise a temperature in the range of from about 160° C. to about 250° C.; and (c) recovering said molecular sieve. |