Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44ce432b65aeefb1e10099423a7efcf2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ca037fd33521b0cda5cd18c26699944c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e3b39029655ed2275bf5af627ec18903 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2383-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-0504 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-16 |
filingDate |
2004-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2472fb5bcbe3dfb995aa6ade84740041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e2e78b7f45f12a0617a248b43f3b4ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6471a6696fd45685b2efe500ce3e568e |
publicationDate |
2007-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2007123628-A1 |
titleOfInvention |
Emulsion composition for silicone rubber, process for producing the same, and process for producing silicone rubber |
abstract |
A silicone rubber emulsion composition comprising (A) 100 parts diorganopolysiloxane having at least two silicon-bonded alkenyl groups, (E) 0 to 60 parts reinforcing silica filler, (B) 10 to 250 parts water containing a smectite clay, (C) 0.1 to 15 parts emulsifier, and (D) a cross-linking agent (e.g., an organohydrogenpolysiloxane) in an amount sufficient for cross-linking component (A) and a catalyst (e.g., a platinum-type catalyst). A method for preparing the aforementioned emulsion composition comprising mixing components (A) and (E) with other components in a high-speed stirrer-equipped mixer. A method of manufacturing a silicone rubber comprising either heating and dehydrating the aforementioned emulsion composition. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011319510-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014502648-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10857758-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113248765-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112321848-A |
priorityDate |
2003-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |