abstract |
A manufacturing method for wear resistant sintered member is provided. The method includes: compacting a raw powder containing a matrix forming powder and a hard phase forming powder into a green compact, the matrix forming powder containing 90 mass % or more of a powder having the maximum particle diameter of 46 μm, and the hard phase forming powder being 40 to 70 mass % with respect to the raw powder; and sintering the green compact. |