Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e643df164d408263905077a4d3016558 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 |
filingDate |
2006-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6fa64caa9e332993d9ebdb92582c4db9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4744da1da8d70b7bfcd32c250d275cf3 |
publicationDate |
2007-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2007073001-A1 |
titleOfInvention |
Rubber composition for tire and tire using the same |
abstract |
A rubber composition for a tire excellent in grip performance and abrasion resistance of a tire and a tire using the same are provided. A rubber composition for a tire comprising a diene rubber and an aromatic vinyl polymer having a glass transition temperature at most 10° C. and a tire using the same. An amount of the aromatic vinyl polymer is preferably 5 to 150 parts by weight based on 100 parts by weight of the diene rubber. |