abstract |
Low melting temperature compliant solders are disclosed. In one particular exemplary embodiment, a low melting temperature compliant solder alloy comprises from about 91.5% to about 97.998% by weight tin, from about 0.001% to about 3.5% by weight silver, from about 0.0% to about 1.0% by weight copper, and from about 2.001% to about 4.0% by weight indium. |