Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a699dc587e9720c5abd9759fd2b2c7b3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cd243f5ceab261e49df9b202a1628a89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_df41bfb96f516e520a01cc7598e74f83 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e1952fca643453e318d811643b5e5684 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2319-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-143 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2321-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-382 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-42 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F136-00 |
filingDate |
2005-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cacad5413e773d185d09cb07e9e10075 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_db3893dee2e75ebde59efd08e25f242a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b5adf0a6b1c1e6b9fc1e7fba32d8d81 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_783fc703124f735b4d622b674109514d |
publicationDate |
2007-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2007060711-A1 |
titleOfInvention |
Silicon-modified crumb rubber composition |
abstract |
The present invention relates to a modified crumb rubber particle having carbon to silicon bonds created by the reaction of the unsaturation in the crumb rubber particle and silicon hydride, with or without the use of a catalyst. Bound silicon content ranges from about 0.1% to 10% by weight. The silicon-modified crumb rubber can be used as is or a reinforcing filler in formulations. Typically the silicon-modified crumb rubber is used in up to 25% by weight of the total rubber present in virgin rubber compositions. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3060586-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11046838-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3947542-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11427702-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11028254-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11155701-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018115715-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014095267-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11396208-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2999585-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11041065-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022234443-A1 |
priorityDate |
2005-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |