http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006251899-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_29ab555a71c7a2e54aaa6fa1afb444f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_741bb450678aff181d301a986224241d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31504 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-249921 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-256 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-2533 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B23-0071 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-266 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-2542 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-256 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-254 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-00 |
filingDate | 2005-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e7a3fd7f5dff27b7d4084170cb54255 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_673e5b035d83af941e987a7fd08959d4 |
publicationDate | 2006-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2006251899-A1 |
titleOfInvention | Process for manufacturing a multilayer article possessing a protective layer |
abstract | A process is provided for fabricating a multilayer article possessing a protective layer which comprises: a) applying a curable protective layer-forming composition to the release coating side of a release liner; b) curing the curable protective layer-forming composition on the release liner; c) forming a plurality of release elements from the structure resulting from step (b), each release element possessing a cured protective layer releasably adhered on one side thereof to the release coating side of the release liner, the other side of the cured protective layer being exposed; d) applying the exposed side of the cured protective layer of a release element to a substrate layer with a quantity of curable adhesive disposed therebetween to provide a curable multilayer article; e) curing the curable multilayer article to adhesively bond the protective layer of its release element to its substrate layer; and, f) separating the cured multilayer article from its release liner to provide a multilayer article possessing a protective layer bonded to a substrate layer. The foregoing process is especially adapted for the manufacture of a high capacity optical information storage medium, in particular, a Blu-ray Disc. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009000727-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008003420-A1 |
priorityDate | 2005-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 58.