Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c69f1fe935647651cf99173c4478dbf0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1c966b2cf3c5786391521e6a8670f077 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0047 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0048 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A24F15-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-004 |
filingDate |
2006-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_56c5673226b56d1c3ecae30f6d3d448d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3ff8291f6de0bb4f0cbd75411f2eaca |
publicationDate |
2006-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2006216644-A1 |
titleOfInvention |
Method for preparing photosensitive aqueous developable coating composition |
abstract |
A method for preparing a photosensitive aqueous developable coating composition is disclosed. The method does not involve a step of drying, pulverizing, and re-dissolving a solid polymer when preparing the coating composition. In addition, dilution of a polymerization solution by a solvent and a separate process for adjusting the viscosity of the polymerization solution are not needed. Therefore, the process for preparing the compositions can be simplified and undercut problems of a patterned edge during development and subsequent edge curl problems after a firing process can be overcome. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2012199192-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8158504-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8482089-B2 |
priorityDate |
2004-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |