Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2a019eaf5d38f18de6fcc4fada9270cc |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2423-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2848 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2250-242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31757 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2255-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2817 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2477-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2255-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2405-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24942 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31913 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-16 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-12 |
filingDate |
2006-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6679cffb9580476eb423c90563f5a241 |
publicationDate |
2006-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2006204736-A1 |
titleOfInvention |
Adhesive tape produced using a hot-melt technique and having an opaque BOPP backing film |
abstract |
The adhesive tape has an adhesive layer of the hot-melt type applied to a backing film based on biorientated polypropylene. This film comprises in succession at least a first layer comprising polypropylene or a mixture of polypropylene resins having a melting point of between 150 and 170° C. and an MFI of between 1 and 5 g/10 min at a temperature of 230° C. and 2.16 kg, an opaque layer comprising a polyethylene-based resin having a melting point of between 120 and 150° C. and an MFI of between 1 and 5 g/10 min at a temperature of 230° C. and 2.16 kg, and a layer of polyamide-resin-based lacquer. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7960024-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010190399-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010189963-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010190398-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8114507-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8147957-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8119549-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8029633-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010186880-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8309478-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8133537-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011206849-A1 |
priorityDate |
2005-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |