abstract |
There is provided a process for producing a modified polyolefin resin, which comprises the step of melt-kneading a blend containing: (A) 100 parts by weight of a polyolefin resin, (B) 0.1 to 20 parts by weight of a compound represented by the following formula (1), and n n(C) 0.01 to 20 parts by weight of an organic peroxide having a decomposition temperature of 50 to 115° C., at which temperature a half-life thereof is 1 minute, n n nwherein R 1 is a hydrogen atom or an alkyl group having 1 to 6 carbon atoms; and R 2 is an alkylene group having 1 to 20 carbon atoms. |