Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C11D17-065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C11D1-146 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C11D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C11D11-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C305-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D17-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61Q19-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C303-42 |
filingDate |
2004-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1472934b08e8cb8a605677940887f536 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f01608b8156e1131445ab3fe51605d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af1799ac81ded4435be70639860ee3cf |
publicationDate |
2005-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2005170993-A1 |
titleOfInvention |
Process for producing a granular anionic surfactant |
abstract |
The invention provides a granular anionic surfactant and a detergent composition blended with the same. Disclosed are a process for producing a granular anionic surfactant, which including stirring particles containing 50 to 100 wt % of an anionic surfactant at a temperature at which the anionic surfactant exhibits thermoplasticity at a stirring Froude number as defined below by equation (i) of 0.1 or more and less than 2.0; a granular anionic surfactant obtained by the process; a granular anionic surfactant having a surface roughness (Ra) of 1.0 μm or less; and a detergent composition comprising the granular anionic surfactant. n n Fr=V /[( R×g ) 0.5 ] (i) n nwherein Fr is Froude number, V is the peripheral speed at the top of a stirring blade [m/s], R is the radius of gyration of a stirring blade [m], and g is the acceleration of gravity [m/s 2 ]. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8207106-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-112007002929-B4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006166852-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010324325-A1 |
priorityDate |
2003-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |