http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004230002-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 |
filingDate | 2003-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c8da12a3ea8e6dfa6d3bba245584feed http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e90d82e0af4fa4e50ab253770247448 |
publicationDate | 2004-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2004230002-A1 |
titleOfInvention | Composition containing ethylene/propylene/diene copolymer and polyalkylene/olefin copolymer |
abstract | A composition suitable for forming a sidewall for a tire includes a rubber composition which includes at least one rubber, an ethylene/propylene/diene terpolymer, and a polyalkylene copolymer. The rubber may include one or more natural or synthetic rubbers, such as butadiene rubbers and isoprene rubbers. The ethylene/propylene/diene terpolymer preferably has an ethylene content of at least 60%. The polyalkylene copolymer may be a copolymer of a polyalkylene and an α-olefin, which is formed in a polymerization reaction involving a single site catalyst. The polyalkylene copolymer preferably has a high degree of crystallinity, being preferably at least about 90% by weight ethylene, with a melting point in the range of 80° C.-120° C. The presence of such a copolymer in the rubber composition markedly increases the resistance to crack growth and formation of cracks in the tire sidewall. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-4230693-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009206511-A1 |
priorityDate | 2003-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 80.