http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004198914-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F255-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-00 |
filingDate | 2004-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bbeacd4719d512447c34d73e2b87be89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_034e63e0c5bea1534de8ac9723720a79 |
publicationDate | 2004-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2004198914-A1 |
titleOfInvention | Process for producing modified polyethylene resin |
abstract | A process for producing a modified polyethylene resin, which comprises the step of melt kneading at least: n (A) 100 parts by weight of a polyethylene resin, n (B) from 0.1 to 20 parts by weight of at least one compound selected from the group consisting of: n (B1) a compound having in its molecule (i) at least one carbon-carbon double or triple bond and (ii) at least one polar group, and n (B2) a compound having in its molecule (iii) an OR group and (iv) at least two specific functional groups, and n (C) from 0.01 to 20 parts by weight of an organic peroxide having a decomposition temperature of from 50 to 115° C., at which temperature a half-life thereof is 1 minute. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008101647-A1 |
priorityDate | 2003-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 502.