http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004087757-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2079-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2379-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2007-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2071-0027 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C71-02 |
filingDate | 2001-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_30614fd9bbedae0ec2cb81a2bfeeadf1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_49c8efcac2632e2d81f07f01e10be4d4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fc87fe13da6214fc7a4cf421dbd6103a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_002192f1eaf7501e1d547223ab573def |
publicationDate | 2004-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2004087757-A1 |
titleOfInvention | Polyimide film and method for production thereof and method for adjusting isotropy thereof |
abstract | To provide a polyimide film having an original film width of at least 500 mm, whose isotropy in a width direction is improved to have uniform properties, which polyimide film has been apt to cause property difference in the width direction by continuous molding. n The polyimide film has an original film width of at least 500 mm and a thickness of at most 50 μm, wherein the maximum value of MOR-c is at most 1.35 and a tensile elastic modulus is at least 5.0 GPa at any part of the film. The polyimide film is prepared by the method which comprises steps of: forming a green sheet containing a volatile component, and heating the green sheet by transferring the same through a furnace with both ends of the green sheet being fixed, wherein at the heating step, the original film has an orientation axis angle θ of a positive value at both ends in the original film width direction, and temperature is lower than the boiling point of a main volatile component in a zone where the original film is transferred for a distance equal to the film width between both fixed ends. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007042167-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7691961-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007071910-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007221096-A1 |
priorityDate | 2000-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 80.