Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2810-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H2401-111 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41N7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65H3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65H27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F32-00 |
filingDate |
2003-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e7d6bbb0a42faa80cee0c3cf47091e1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_100bdf04b3d44f2ddbb81b98306e5888 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cd53fb906f0731339bdff95a6a25f4ee |
publicationDate |
2004-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2004082725-A1 |
titleOfInvention |
Elastomer composition and rubber roller composed thereof |
abstract |
A rubber roller ( 1 ) is formed by molding an elastomer composition not less than 250 μs nor more than 400 μs in a T2 relaxation time (spin-spin relaxation) of a bound rubber formed between a rubber or/and a thermoplastic elastomer and a reinforcing filler. It is preferable to use EPDM as the rubber or/and the thermoplastic elastomer, carbon black as the reinforcing filler, and crosslink the EPDM with an organic peroxide. It is also preferable that the T2 relaxation time (spin-spin relaxation) of the bound rubber formed between the rubber or/and the thermoplastic elastomer and the reinforcing filler is more than a T2 relaxation time of a bound rubber of the rubber or/and the thermoplastic elastomer to which the reinforcing filler is not added by not less than 150% nor more than 300%. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9371426-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8986182-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102245685-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011034308-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011034598-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015189870-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006154002-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007073442-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7812093-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11124626-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010067232-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010144916-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007142554-A1 |
priorityDate |
2002-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |