http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004044151-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C11D3-378 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D3-37 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-04 |
filingDate | 2003-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a9f2296f0d5ea7aadf4d7b9d4c34d492 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ce7691784075dfbc97074861aac69b0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_499864276b3da789c9e20a3f7a766005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd18d44a0fbc25cc4a9c0b104ebe1f51 |
publicationDate | 2004-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2004044151-A1 |
titleOfInvention | Sulfur-containing poly (unsaturated carboxylic acid) and its uses and production process |
abstract | There are disclosed a novel sulfur-containing poly(unsaturated carboxylic acid) and its uses and production process. A sulfur-containing poly(unsaturated carboxylic acid) having a weight-average molecular weight (Mw) of 500 to 4,500 and a molecular weight distribution (Mw/Mn) of not more than 2.5 is obtained by a production process comprising the step of polymerizing an unsaturated carboxylic acid in the presence of a polymerization initiator to thereby obtain the poly(unsaturated carboxylic acid), wherein: a combination of a persulfate and a bisulfite is used as the polymerization initiator, wherein the polymerization initiator is adjusted in such a manner that: the total amount of the polymerization initiator as used is not smaller than 10 g equivalents per 1 mol of the unsaturated carboxylic acid as used, and the amount of the bisulfite accounts for not smaller than 8 g equivalents of the total amount of the polymerization initiator as used; and the polymerization temperature is controlled so as to be in the range of 25 to 99° C. This polymer is used as an essential component of a detergent builder and a kaolin dispersant. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007149806-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7399818-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008318832-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005209410-A1 |
priorityDate | 2002-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 156.