abstract |
A resin composition for high-frequency bonding with a dielectric loss tangent of 0.03 or higher at a frequency of 40 MHz, containing a thermoplastic resin having a melting point of 80° C. to 200° C. in an amount of 70% to 99% by volume, based on the total volume of the composition, and a conductive material having a volume resistivity of 10 −2 Ω.cm or lower in an amount of 30% to 1% by volume, based on the total volume of the composition. |