Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J2211-42 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7734 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-595 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0007 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-00 |
filingDate |
1999-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_89f0ced4ac06699c908effd6fa09ba27 |
publicationDate |
2002-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2002106446-A1 |
titleOfInvention |
Process for forming a pattern of fluorescent substrate and plasma display panel |
abstract |
A resin composition (A) layer, comprising an acrylic polymer (a) having a weight average molecular weight of 10000 to 300000 and an acid number of 80 to 250 mgKOH/g and a fluorescent substance (b), and a photosensitive resin composition (B) layer are formed inside the cell, and then they are exposed, developed and baked. By the process of the present invention the fluorescent substance can be effectively and uniformly formed on the side and bottom wall of the cell. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8044572-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007257597-A1 |
priorityDate |
1998-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |