http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2001023278-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2800-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2810-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B13-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F255-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-244 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-00 |
filingDate | 2001-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c12d45172b4597f376a03310c75bf51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d4156d023fb35cbcb27aaf5e59855895 |
publicationDate | 2001-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2001023278-A1 |
titleOfInvention | Elastomers with improved processability |
abstract | A process for improving the green strength of ethylene/α-olefin/diene polymers is described comprising (A) selecting an ethylene/(αolefin/diene polymer having a Mooney viscosity at 125 C up to about 80 and a percent gel (% gel) up to about 30 percent and (B) partially crosslinking the ethylene/α-olefin/diene polymer selected in step (A) to make a modified ethylene/α-olefin/diene polymer satisfying the equations MV≦100 and n W ≤ ( MS 2 - MS 1 MS 1 ) n n wherein MV is the Mooney viscosity of the modified polymer, MS 1 is the melt strength in centiNewtons of the polymer selected in step (A) at 110 C, when formulated according to ASTM D3568#2, MS 2 is the melt strength in centiNewtons of the modified polymer produced by step (B) measured under the same conditions, and W is 0.3. Modified ethylene/α-olefin/diene polymers obtainable according to the above process or satisfying the equation: n MS 2 ≥ ( MV X + % gel Y ) Z n n is also described in which MS 2 , MV and % gel of the modified polymer are defined as defined above, X is 50, Y is 20, and Z is 40. Further described is a process for making an article comprising an ethylene/α-olefin/diene polymer and intermediates for making the modified ethylene/α-olefin/diene polymers. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005016980-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11485298-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10589452-B2 |
priorityDate | 1997-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 237.