Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d79a3714d75520adeea100b7ed428a77 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-92 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B20-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B15-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B19-095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B29-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-004 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B15-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B20-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B19-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B29-06 |
filingDate |
2018-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2022-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d41a93456f35d20161990830ce2ea21d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5be7114649c75ca4d09ac82c369b6c7c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_443667799ce98f1bcd90ed6e21d78c54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_282560e1f108d3c8816184b56fa5d378 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c0035ea6b88dae04014e2af166464f60 |
publicationDate |
2022-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-11473209-B2 |
titleOfInvention |
Quartz glass crucible and manufacturing method thereof |
abstract |
In an exemplary embodiment, a quartz glass crucible 1 includes: a cylindrical crucible body 10 which has a bottom and is made of quartz glass; and crystallization-accelerator-containing coating films 13 A and 13 B which are formed on surfaces of the crucible body 10 so as to cause crystallization-accelerator-enriched layers to be formed in the vicinity of the surfaces of the crucible body 10 by heating during a step of pulling up a silicon single crystal by a Czochralski method. The quartz glass crucible is capable of withstanding a single crystal pull-up step undertaken for a very long period of time, such as multi-pulling, and a manufacturing method thereof. |