http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11329265-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f1192a135e4bc40a5f201a9646f20172 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0404 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-624 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-139 |
filingDate | 2018-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b27eaf075f08e90f853c2a2b63a014b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c0f1753d83a5df615e3e6035c86dffb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d84bace9850ed0c5f3e07864415c3de http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d52c1bc7345d67b791aa43a812464bd4 |
publicationDate | 2022-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-11329265-B2 |
titleOfInvention | Method for producing battery electrode |
abstract | Provided is a means capable of improving the flatness of a surface of an electrode active material layer in which an electrode active material slurry without assuming addition of a binder.Upon producing a battery electrode which has a current collector and an electrode active material layer disposed on a surface of the current collector and containing an electrode active material, in a coating step of coating an electrode active material slurry in which the electrode active material is dispersed in a solvent on the surface of the current collector to form the electrode active material layer, an electrode active material slurry which has flow characteristics that a region A in which a shear stress is not increased according to an increase in shear rate is present and a region B in which a shear stress is increased and an increase rate thereof is decreased according to an increase in shear rate is present in a region having a shear rate larger than that of the region A, in a shear rate (horizontal axis)-shear stress (vertical axis) curve of the electrode active material slurry, is used as the electrode active material slurry, and, coating of the electrode active material slurry is performed at a coating rate at which the shear rate at the time of coating is a value in which a shear stress equal to or more than a yield stress of the electrode active material slurry is applied in the coating step. |
priorityDate | 2017-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |