http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11292214-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f1192a135e4bc40a5f201a9646f20172 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2791-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2063-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C70-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C33-0038 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-44 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C70-48 |
filingDate | 2018-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_832b8b7ba53b998c3b503f95ebd80aff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da3ebe630d02d2f72428381ea1c1c6ee |
publicationDate | 2022-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-11292214-B2 |
titleOfInvention | Method for molding composite material and device for molding composite material |
abstract | A method for molding a composite material and a device for molding a composite material are provided which are able to suppress the occurrence of voids in a composite material and improve the mechanical characteristics and appearance quality of the composite material. In the method for molding a composite material (10), a seal region (270) including a cavity (250) in which a reinforcing base material (11) is disposed and an outer peripheral region (260) that communicates with an outer periphery of the cavity is air-tightly sealed by means of a first sealing member (310). Then, an operation of suctioning a gas from the outer peripheral region to evacuate the gas in the seal region is started, and a resin (12) is injected into a part of the cavity. Next, a mold (200) is clamped to provide a liquid-tight seal between the cavity and the outer peripheral region by means of a second sealing member (320) while pressing the resin to fill the cavity with the resin. After that, the operation of suctioning the gas from the outer peripheral region is stopped. |
priorityDate | 2017-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419505877 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3365 |
Total number of triples: 28.