abstract |
Provided is a method of producing a polycarbonate resin pellet containing a polycarbonate resin serving as a component (A), a silicone compound serving as a component (B), and an ester of an aliphatic carboxylic acid having 12 to 22 carbon atoms and glycerin serving as a component (C), the production method including a step including introducing a blend containing the component (A), the component (B), and the component (C) into an extruder, and melt-kneading the blend in the extruder under such a condition that a temperature of a molten resin at an outlet of the extruder is 260° C. or more and 325° C. or less, followed by extrusion molding to provide a polycarbonate resin pellet, the resultant polycarbonate resin pellet containing 0.01 part by mass or more and 0.25 part by mass or less of the component (B), and 0.015 part by mass or more and 0.25 part by mass or less of the component (C) with respect to 100 parts by mass of the component (A). |