An electrostatic-image developing toner includes toner particles, layered compound particles, and inorganic particles. The inorganic particles have an average circularity of 0.910 or more and 0.995 or less. A ratio Da/Db of a number-average particle size Da of the layered compound particles to a number-average particle size Db of the inorganic particles is 1.2 or more and 43 or less.