Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B2203-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B2203-017 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B2203-013 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B3-84 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B3-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B3-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B3-28 |
filingDate |
2016-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2021-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_62184f85a286edb6a7c0ef323fd79ac5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cfb76bb469a323c10d2246c8973948a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f524141e68f42a285ff3cd78b847e3e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1aab1dc3900ab20804c6eca787ccd509 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c11d915a21f1e08aa7ac529421794e9 |
publicationDate |
2021-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-10964445-B2 |
titleOfInvention |
Heating element and manufacturing method therefor |
abstract |
The present disclosure relates to a method for manufacturing a heating element, which includes the steps of: preparing a first bonding film; forming a conductive heating pattern on the first bonding film; and laminating a second bonding film and a transparent substrate on the first bonding film, where the second bonding film is disposed on a surface opposite to the surface provided with the conductive heating pattern of the first bonding film, and the conductive heating pattern is formed by using an adhesive film having an adhesive strength decrement of 30% or greater by an external stimulus based on adhesive strength before the external stimulus. |