Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e0bf0928b608797b70bbc2b91c7e52e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2280-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4854 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-244 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3206 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4018 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-664 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6674 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4216 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-7671 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 |
filingDate |
2016-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2021-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce700fa4aa66c3504abc85cd4873a580 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59741fbeda97d6d5d2127056395d0bb4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_058b82d926abf377c131df64f98b874d |
publicationDate |
2021-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-10907006-B2 |
titleOfInvention |
TPU shrink material |
abstract |
The present invention relates to a method for producing a molded body (MB) comprising the production of a thermoplastic polyurethane, the production of a molded body (MB*) from the thermoplastic polyurethane, heating the molded body (MB*) to a temperature below the temperature at which there is permanent deformability of the molded body (MB*), and above the switching temperature of the thermoplastic polyurethanes, elongating the heated molded body (MB*) with obtention of a molded body (MB), and cooling the molded body (MB) to a temperature below the switching temperature of the thermoplastic polyurethane, and the molded body obtained or obtainable by such a method. The present invention further relates to a thermoplastic polyurethane with shape memory and the use of a thermoplastic polyurethane for producing a molded body with shape memory effect in a temperature range from 0° C. to 130° C. |
priorityDate |
2015-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |