abstract |
The antifouling film includes a polymer layer that includes on a surface thereof an uneven structure provided with multiple projections at a pitch not longer than a wavelength of visible light. The polymer layer has a proportion of the number of fluorine atoms relative to the sum of the numbers of carbon atoms, nitrogen atoms, oxygen atoms, and fluorine atoms of 33 atom % or more on the surface of the uneven structure and of 3 atom % or less on average in a region 90 to 120 nm deep from the surface of the uneven structure. The polymer layer has a proportion of the number of nitrogen atoms relative to the sum of the numbers of carbon atoms, nitrogen atoms, oxygen atoms, and fluorine atoms of 4 atom % or less on average in a region 90 to 120 nm deep from the surface of the uneven structure. |