http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10544287-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2296 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-006 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 |
filingDate | 2015-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1843496e13f9d2f774be66a2245149c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa238f8b66f1aa1d62c757dd65ef7476 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_874e11699a853214169c6af2b0f358df |
publicationDate | 2020-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-10544287-B2 |
titleOfInvention | Rubber composition for tire |
abstract | The rubber composition of the present invention is prepared by mixing a rubber component (A), zinc oxide (B), and a co-condensate (C) having a softening point of 150° C. or lower and containing a p-tert-butylphenol-derived constituent unit represented by the following formula (1), an o-phenylphenol-derived constituent unit represented by the following formula (2) and a resorcinol-derived constituent unit represented by the following formula (3), wherein the nitrogen adsorption specific surface area (N 2 SA) of the zinc oxide (B) measured according to the BET method is 6 m 2 /g or more and 110 m 2 /g or less, the mixing amount of the zinc oxide (B) is 5 parts by mass or more and 13 parts by mass or less based on 100 parts by mass of the rubber component (A), and the mixing amount of the co-condensate (C) is 0.1 parts by mass or more and 10 parts by mass or less based on 100 parts by mass of the rubber component (A). The co-condensate (C) is usable as a replacement for p-tert-octylphenol and p-nonylphenol, has a softening point lower than the maximum temperature in a rubber processing step, and has excellent dispersibility in rubber. |