abstract |
A joined body 20 includes a porous ceramic 22 made of porous ceramic, a metal member 24 made of a metal, and a joint 30 formed of an oxide ceramic that penetrates into pores 23 of the porous ceramic 22 and joins the porous ceramic 22 to the metal member 24 . The penetration depth of the oxide ceramic into the pores of the porous ceramic is preferably 10 μm or more, and more preferably 15 to 50 μm. The joined body 20 may be produced through a joining step of forming a joint by placing a metal raw material between a porous ceramic and a metal member and firing the metal raw material in the air at a temperature in the range of 400° C. to 900° C., where an oxide ceramic produced by oxidation of the metal raw material penetrates into the pores of the porous ceramic in the joint. |