abstract |
An amorphous mesoporous alumina with a median mesopore diameter by volume of 16 nm or more, a mesopore volume of 0.5 mL/g or more, and a total pore volume of more than 0.75 mL/g. A process for preparing said alumina, comprising:n a) precipitating a basic precursor and an acidic precursor, at least one of which comprises aluminum, at a pH of 8.5 to 10.5, a temperature of 20° C. to 90° C. and for 2 minutes to 30 minutes, with a state of advance of 5% to 13%; b) heating the suspension; c) a second precipitating by adding another basic precursor and acidic precursor, at least one of which comprises aluminum, at a pH of 8.5 to 10.5, a temperature of 40° C. to 90° C. and for 2 to 50 minutes, with a state of advance of 87% to 95%; d) filtration; e) drying; f) shaping; g) heat treatment. |