Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5f7f120efe096284c7389702c969cf3d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2200-0607 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2309-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-34 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-247 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L15-005 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-02 |
filingDate |
2016-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2018-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1bc80cae0add948b2c81e9b1096df150 |
publicationDate |
2018-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-10005895-B2 |
titleOfInvention |
Cross-linked rubber product |
abstract |
A cross-linked rubber product for a fuel seal is obtained by cross-linking a nitrile rubber composition including a nitrile rubber (A) containing 25 to 80% by weight of α,β-ethylenically unsaturated nitrile monomer units (a1), 20 to 75% by weight of conjugated diene monomer units (a2), and 0 to 30% by weight of cationic monomer units and/or monomer units capable of forming a cation (a3), and having a compression set ratio of 20% or less after being compressed in an atmosphere of 100° C. for 70 hours, and an inorganic filler (B) having an aspect ratio of 30 to 2,000. The content of the inorganic filler (B) is from 1 to 200 parts by weight with respect to 100 parts by weight of the nitrile rubber (A). The cross-linked rubber product is obtained by subjecting the nitrile rubber composition to secondary vulcanization at 100 to 150° C. for 1 to 24 hours. |