abstract |
The polyamide resin composition of the present invention comprising: a semi-aromatic polyamide (A) having a melting point of 280 to 320 ℃, an aliphatic polyamide (B), 5 to 30 % by mass of a phosphinic acid metal salt (C), 5 to 60% by mass of a reinforcing material (D), 0.1 to 8% by mass of a carbonate metal salt (E), and 0.01 to 3 % by mass of a fatty acid barium salt (F); the total content of (A) and (B) is 30 to 85% by mass, and the mass ratio (A/B) of (A) and (B) is 90/10 to 40/60. |