Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_962adbf7d50e742218f3d536a63df612 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 |
filingDate |
2017-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2021-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0053c0e45d88e69244738e68186feef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a33f80e7068ffaaa02a0b62b97d5d112 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_338526fd9e4037d9b5c6e9b36ede2275 |
publicationDate |
2021-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-I740991-B |
titleOfInvention |
Method for manufacturing thin-film liquid-repellent layer, and thin-film liquid-repellent layer |
abstract |
The present invention relates to a method for manufacturing a thin film liquid-repellent layer, which sequentially has the step (1): using a component (A) containing a tetrafunctional silane compound with a specific structure and a component with a trifunctional silane compound with a specific structure The step of forming a cured film of the liquid-repellent composition of (B), and step (2): the step of removing the surface of the cured film obtained in the aforementioned step (1) to thin the film. The present invention relates to a method of manufacturing The manufactured thin-film liquid-repellent layer, and a thin-film liquid-repellent layer, is a cured product of component (A) and component (B), and the thickness is less than 8nm. |