http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I732820-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_98ec0629c8a506ce664ac51ffe289487 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-00 |
filingDate | 2017-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b015f67a145d70a0448bef3521cdef9d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c87641943e4e54ccbcbfbdfdb48d315 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3bbdba0dcfade3b9a0140d5f050a6d7b |
publicationDate | 2021-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-I732820-B |
titleOfInvention | Fully aromatic liquid crystal polyester resin and its manufacturing method |
abstract | The subject of the present invention is to provide a wholly aromatic liquid crystal polyester resin with high mechanical strength, excellent filling properties, blistering resistance, and low warpage. The wholly aromatic liquid crystal polyester resin of the present invention is characterized in that it contains structural units (I) to (V) represented by the following formulas (I) to (V), The composition ratio (mol%) of the structural units (I) to (V) in the above aromatic liquid crystal polyester satisfies the following conditions: 15 mol%≦structural unit (I)≦35 mol% 5 mol%≦ Structural unit (II) ≦ 15 mol% 21 mol% ≦ structural unit (III) ≦ 29 mol% 1 mol% ≦ structural unit (IV) ≦ 9 mol% 25 mol% ≦ structural unit (V) ≦40 mol% structural unit (I) + structural unit (II) + structural unit (III) + structural unit (IV) + structural unit (V) = 100 mol%, and the above-mentioned wholly aromatic liquid crystal polyester resin The melting point is above 320°C. |