Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3597e746ed8bd1a07ac7eb3bfe5c8075 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M2101-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M2200-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M13-395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M13-35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-263 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-263 |
filingDate |
2019-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2021-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31151eab49199636c1bbe614aa61b480 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8d3a5a986ca062a396ec8e270cf44e7e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36db078e194bb05e3047637318d0b19d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c52a2f9794c7fe7d47d864b89056832 |
publicationDate |
2021-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-I718683-B |
titleOfInvention |
Manufacturing method of hydrophobic yarn |
abstract |
A manufacturing method of a hydrophobic yarn includes performing a hydrophobic treatment to a polyester yarn. The polyester yarn is soaked in a hydrophobic treatment solution and treated by a pressure cycling at a temperature of 25℃ to 75℃ and under a pressure of 1 to 5kgf/cm 2 to form a hydrophobic yarn. The hydrophobic treatment solution includes 5 parts by weight to 45 parts by weight of a fluorine-free water repellent, 0.5 parts by weight to 5 parts by weight of a bridging agent, nand 50 parts by weight to 95.5 parts by weight of a solvent. |