http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I717109-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4a8faea375370b67c9d71e67db32bcd |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L23-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 |
filingDate | 2019-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-01-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a946b80191a8dcc017bf994377341df http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6f925869d4ebcd2fb4d679b6cc1e0b3 |
publicationDate | 2021-01-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-I717109-B |
titleOfInvention | Sealing material resin composition for high frequency and semiconductor device |
abstract | The present invention is a sealing material resin composition for high frequency, which contains (A) epoxy resin, (B) benzox resin, (C) phenol hardener, (D) hardening accelerator and (E) inorganic Filler, andnThe degree of hardening at 120 seconds measured by the following measuring conditions is 0.35 or more and less than 0.55, and the degree of hardening at 150 seconds is 0.50 or more and less than 0.75, nThe relative dielectric constant of the cured product of the above resin composition at 70 GHz is 3.40 or less.n(Measurement condition of hardening degree)nUsing a vulcanizer, when the above resin composition is cured under the conditions of a mold temperature of 175°C and a molding time of 300 seconds, the torque values at the molding time of 120 seconds and 150 seconds are measured, and the following formulas (1) and 2) Calculate the degree of hardening of each.nHardness 120 n= Torque value 120 n/Torque value 300 n(1)nHardness 150 n= Torque value 150 n/Torque value 300 n(2) |