abstract |
An optical laminate, its manufacturing method, a front panel and an image display device; [1] An optical laminate having a substrate film, a transparent conductive layer and a surface protective layer in sequence, and the average value of the surface resistivity is 1.0× 10 7 ~10 10 Ω/□, the standard deviation σ is 5.0×10 8 Ω/□ or less; [2] An optical laminate with a cycloolefin polymer film, a transparent conductive layer and a surface protective layer in sequence. The ratio of the thickness to the overall thickness is 80~95%, and the elongation measured under specific conditions is 5.0~20%; [3] An optical laminate with a cellulose base film and a stabilizing layer in sequence And the conductive layer, the average value of the surface resistivity is 1.0×10 7 to 10 12 Ω/□, and the standard deviation σ is divided by the average value to obtain a value of 0.20 or less. |