http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I699406-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_617fd97d8122be87eccd6368bef7ac19 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F21V7-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F21V7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F21S2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F21K2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F21V7-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13357 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F21V7-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 |
filingDate | 2016-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_40db1e2846861a4273fbf61cdacbd85a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d7edec51b52c36f6ee7537013942057c |
publicationDate | 2020-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-I699406-B |
titleOfInvention | White reflective film |
abstract | The subject of the present invention is to provide a white reflective film that can sufficiently inhibit adhesion to the light guide plate under normal conditions, and is a water-based coating layer at the same time can inhibit adhesion to the light guide plate even in a humid and hot environment, and The recyclability of the film is high. For such a problem, the present invention is a white reflective film, which is a white reflective film having a coating layer formed by a water-based coating liquid on the surface of the reflective film, and the water-based coating liquid contains a solid binder resin and particles As the main component, it is characterized in that the surface of the coating layer has protrusions formed by the particles, and the number of protrusions with a height of 5 μm or more is 10 4 pieces/m 2 to 10 10 pieces/m 2 , The adhesive resin contains a copolymerized polyester resin with a glass transition temperature Tg of 100°C to 120°C and is 5% to 50% by mass based on the quality of the adhesive resin, and the adhesive resin contains a glass transition temperature Tg of The thermoplastic resin below 100°C is 50% to 95% by mass based on the mass of the binder resin. |
priorityDate | 2015-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 65.