Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G79-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F7-0838 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F7-1804 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F7-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 |
filingDate |
2015-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2020-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_74ee8b806ab7677f81e9f6f991aabb4a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d5e2b368e22848b0506853aa97da95d3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8db40c05260f87704b39c87250424ef4 |
publicationDate |
2020-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-I683858-B |
titleOfInvention |
Transparent film |
abstract |
An object of the present invention is to achieve both water-oil repellent and heat resistance and light resistance. The transparent film of the present film comprises a polysiloxane structure and a trialkylsilyl group-containing chain that boned to part of silicon atoms constituting the polysiloxane structure, wherein the alkyl group of the trialkysilyl group-containing chain may be substituted with a fluoroalkyl group. If an initial dynamic contact angle of liquid droplets on the transparent film is A 0 , a contact angle after standing for 24 hours at 200℃ is B H , a contact angle after irradiating with a xenon lamp having power of 250W for 100 hours is B L , then satisfying at least one of the following formulas: (B H - A 0 ) / A 0 × 100 (%) ≧ -27(%) (B L - A 0 ) / A 0 × 100 (%) ≧ -15(%). |