Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L79-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-621 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-04 |
filingDate |
2016-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2019-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87bb3e78a75a173586cc1295d23199d6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_289e8748cb5c9417b1cc93c3818a4f46 |
publicationDate |
2019-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-I677534-B |
titleOfInvention |
Liquid resin composition |
abstract |
The object of the present invention is to provide a hardened material that has less thermal decomposition (weight reduction) even if it is left at a high temperature of 200 ° C to 250 ° C for a long period of time, and has excellent mechanical properties even in a high temperature and high humidity environment. Reliable resin composition.nn n n The solution is characterized by (A) a cyanate ester compound having two or more cyano groups in one molecule, (B) a phenol hardener containing a resorcinol-type phenol resin, (C) an epoxy resin, and (D) In the liquid resin composition formed by the hardening accelerator, (A) a cyanate ester in a total of 100 parts by mass of (A) a cyanate ester compound, (B) a phenol hardener, and (C) an epoxy resin. The liquid resin composition in which the ester compound has a mass of 30 to 80 parts by mass. |
priorityDate |
2015-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |