Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e620e98a4fcbc02d1a96a9c379aeceea |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09G1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-1415 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-141 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-146 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-14 |
filingDate |
2014-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2018-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f139bf99de548f40e7692de0457d2900 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bdf8c1b41591736be72fb445219b35b8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_779495ad15ebf917238fd95d576d3f40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17e31af50fae9f8810213bae22bf9f23 |
publicationDate |
2018-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-I644862-B |
titleOfInvention |
Process for preparing bismuth sol materials |
abstract |
A process for preparing a cerium sol material capable of controlling the obtained particle size, more specifically, using a potassium hydroxide process to obtain a cerium sol material having a single peak of an average particle size distribution. |
priorityDate |
2013-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |